Material |
Environment |
Test Item |
Typical Value |
Copper Wire | 20℃ | Resistance | 1.55×10ˉ³Ω/m |
Coke Coated Layer | 23℃ | Resistivity | 0.5Ω.cm |
Carbon Content | 99.6% | ||
Acid and Alkali Resistant Layer | 23℃ | Fracture Strength | 980N |
Abrasion Resistant Layer | Stay in different electrolyte environments for six months | Changes of tensile strength less than 20% |
Technical Parameters |
TB39-52 |
Anode Diameter |
39±2mm |
MMO/Ti Anode Wire Diameter |
≥0.8mm |
Anode Design Life |
≥40years |
Anode Consumption (Including Filling) |
≤6mg/A.a |
Output Current (Maximum) |
1500mA/m |
Coating Thickness of Metal Oxide |
≥ 6g/m2 |
Resistivity of Mixed Metal Oxides |
10-5Ω.cm |
Contact Resistance of Anode and Cable Joint |
≤1.0 mΩ |
Anode Resistance |
≤0.007Ω∕m |
Content of Coke Breeze Filler |
≥ 98% |
Coke Breeze Resistance |
≤0.55 Ω·cm |
Fabric Jacket Tube |
Anticorrosion,permeable |
Fabric Jacket Mesh |
Wearproof,anti environmental temperature variability |
Anode Weight |
≥1.3kg/m |
Anode Length(Each Unit) |
500m(or made to order) |